HiPIMS induced a facile synthesis of Ti3SiC2 MAX phase coating
编号:186 访问权限:PARTICIPANT_ONLY 更新:2025-04-15 09:50:26 浏览:294次 张贴报告

报告开始:2025-05-10 17:45

报告时间:15min

所在会场:[V] 成果展及posters [V1] posters

暂无文件

摘要
Ti3SiC2, as a type of the MAX phase, possesses a unique nano-layered structure and exceptional amalgamation of metallic and ceramic, facilitating its potential application as a protective coating used in harsh high-temperature environment. However, the extremely narrow phase-forming region makes it difficult to prepare Ti3SiC2 MAX phase with high purity. In this study, the Ti3SiC2 MAX phase coatings on Ti-6Al-4V substrates were successfully synthesized through a two-step method involving High Power Impulse Magnetron Sputtering (HiPIMS) deposition followed by vacuum annealing at 850 °C for 90 min. The microstructural evolution of the coatings before and after annealing was meticulously examined, and the phase transition of the Ti-Si-C coating during annealing was comprehensively elucidated through X-ray diffraction (XRD) and differential scanning calorimetry (DSC) analyses. The crystallization pathway of Ti3SiC2 during annealing treatment comprises two stages: an initial stage starting from 550 °C, involving the formation of Ti5Si3 interphases, followed by a subsequent stage starting from 750 °C, transitioning to the Ti3SiC2 MAX phase. Additionally, the resulting Ti3SiC2 MAX phase coatings exhibited a remarkable hardness of 25.33 GPa and demonstrated significant corrosion resistance in a 3.5 wt.% NaCl solution, highlighting their potential for applications in demanding environments.
关键词
Ti3SiC2 coating,HiPIMS,Structural evolution,Mechanical property,Anti-corrosion
报告人
许钰玺
中国科学院宁波材料技术与工程研究所

发表评论
验证码 看不清楚,更换一张
全部评论
重要日期
  • 会议日期

    05-09

    2025

    05-11

    2025

  • 05-11 2025

    注册截止日期

  • 05-14 2025

    摘要截稿日期

  • 05-14 2025

    初稿截稿日期

  • 08-07 2025

    报告提交截止日期

主办单位

中国机械工程学会表面工程分会

承办单位

天津大学
中国地质大学(北京)
海南大学
北京科技大学